Dissimilar Materials Welding
Mostrando 1-12 de 15 artigos, teses e dissertações.
-
1. Effects of Geometrical Feature on Microstructures and Mechanical Properties of Refill Friction Stir Spot Welding 6061 Aluminum Alloy
Refill friction stir spot welding (refill FSSW) is a solid state joining technology developed and patented by Helmholtz-Zentrum Geesthacht. Refill FSSW is a welding process suitable for spot joining lightweight materials in similar and dissimilar joint configuration. The result is a spot welded in lap configuration with minimal material loss and a flat surfa
Mat. Res.. Publicado em: 17/01/2020
-
2. Towards Qualification of Friction Stir Welding to AA5083-O and AA5052-O Aluminum Alloys
Friction Stir Welding (FSW) is an excellent alternative for joining dissimilar and similar materials in comparison to conventional welding processes. In this sense, this work aims at qualifying FSW to similar AA5083-O and AA5052-O aluminum alloys, with 6.35 mm thickness, in a CNC machining center. Therefore, four welding experiments were undertaken. At first
Mat. Res.. Publicado em: 13/01/2020
-
3. Resistência à Corrosão de Juntas Dissimilares dos Aços AISI 316L e da Liga Inconel 718
Resumo A soldagem dissimilar (Dissimilar Metal Welds – DMWs), união de dois diferentes materiais metálicos, tem muitas aplicações industriais, com destaque para trocadores de calor nas usinas nucleares. Portanto, devem resistir à corrosão e a esforços mecânicos, entre outros requisitos. Neste trabalho foi abordada a susceptibilidade à corrosão d
Soldag. insp.. Publicado em: 21/10/2019
-
4. Experimental Thermal Analysis in Rotary Friction Welding of Dissimilar Materials
ABSTRACT: Rotary friction welding process (RFW) is one of the most used processes in the world for manufacturing bimetallic components that require high mechanical strength. All process occurs in solid state at temperatures below the melting point of the involved materials, having as the main bonding mechanisms the diffusion and mechanical mixture. The purpo
J. Aerosp. Technol. Manag.. Publicado em: 23/09/2019
-
5. Erratum: Effect of Residual Stresses of GTA Welding for Dissimilar Materials
Mat. Res.. Publicado em: 18/07/2019
-
6. Uma nova abordagem para a medição da diluição de soldagem, baseada nos pontos de inflexão de um Contorno Ativo
RESUMO Em diversas aplicações, com ênfase nos processos de soldagem dissimilar, a diluição, em conjunto com outros fatores, pode afetar as propriedades mecânicas dos materiais soldados, sendo assim, capaz de gerar falhas durante as condições normais de serviço. Deste modo, a taxa de diluição geralmente é calculada a partir da análise de imagens
Matéria (Rio J.). Publicado em: 20/05/2019
-
7. Avaliação Microestrutural e Resistência à Corrosão de uma Junta Dissimilar entre um Aço de Alta Resistência e Baixa Liga e Aço um Inoxidável Duplex
Resumo A união entre materiais dissimilares tem sido amplamente aplicada na indústria de petróleo e gás. Em geral, este tipo de soldagem é mais sensível às diferenças de composição química existente entre os metais envolvidos. Diante dessa perspectiva, este trabalho tem por objetivo avaliar, por união autógena, a microestrutura de uma junta sold
Soldag. insp.. Publicado em: 16/05/2019
-
8. Effect of Residual Stresses of GTA Welding for Dissimilar Materials
The purpose of the present work is to understand the evolution of residual stresses in weldments. The study made to weld the multipass dissimilar of Nickel-based superalloy Inconel 625 and stainless steel 316L using Continuous Current Gas Tungsten Arc Welding (CCGTAW) and Pulsed Current Gas Tungsten Arc Welding (PCGTAW) process employing ERNiCrMo-3 and ERNiC
Mat. Res.. Publicado em: 25/06/2018
-
9. Effect of Heat Input on the Mechanical Behaviour of Al-Cu FSW Lap Joints
Dissimilar Al-Cu joints are desirable due to the combination of the good electrical and thermal properties of copper with the economic advantages of aluminium. However, different chemical, mechanical and thermal properties turn dissimilar welding into a challenge with traditional fusion welding techniques. Friction stir welding appears to be a good alternati
Mat. Res.. Publicado em: 28/05/2018
-
10. Influence of Interlayer Thickness (Zn) on the Properties of Al 7020 FSW Joints
The use of lightweight materials in the production of cryogenic tanks, spacecraft body etc. are becoming the need to develop dissimilar metal FSW joints. Friction stir welding (FSW) is a novel and inspired light metal joining process since it is not involved with the melting of the parent metal. In this work, two Aluminium 7020 plates were welded with Zn as
Mat. Res.. Publicado em: 10/06/2016
-
11. Investigation on AA5083/AA7075+Al2O3 Joint Fabricated by Friction Stir Welding: Characterizing Microstructure, Corrosion and Toughness Behavior
The effects of Al2O3 reinforcements on microstructure, corrosion and toughness properties of dissimilar aluminum alloys joint fabricated by friction stir welding (FSW) technique were explored in this research. AA5083-H116 and AA7075-T6 were selected as the primary base materials. FSW was conducted with and without reinforcing particles through the joint line
Mat. Res.. Publicado em: 2015-12
-
12. Estudo de uniões dissimilares alumínio-soldas por "Solda Ponto por Fricção e mistura mecânica com preenchimento do furo" (Friction Spot Welding - FSpW)
O presente trabalho estuda uniões entre chapas de aço DP600 e chapas das ligas de alumínio AA 6181¿T4 e AA 5754¿H22, obtidas através do processo Friction Spot Welding (FSpW). A soldagem de materiais dissimilares é um dos grandes desafios para a engenharia, pois as propriedades de distintos materiais são muito diferentes na maioria das vezes, o que di
IBICT - Instituto Brasileiro de Informação em Ciência e Tecnologia. Publicado em: 2012