49. Alteração microestrutural do fio de aço inoxidavel 316L, apos deformação e implante no tecido muscular de rato : estudo macroscopico, metalografico e microscopia eletronica de varredura
Stainless steel 316L wire, straight or deformed by torsion, was analysed through a stereoscopic microscope. scanning electron microscope and metallography. Torsion enhanced segregation lines, deformed the surface and generated tension in the internal structure. After implantation in rat muscle, the twisted wire presented lack of cohesion between metal grains
Publicado em: 1992