Validação em laboratório de método analítico para determinação do teor de adipato e ftalato de di-(2-etil-hexila) utilizados como plastificantes em filmes flexíveis de PVC

The validation of analytical methods was carried out for di-(ethylhexyl) phthalate (DEHP) and adipate (DEHA) the determination of in PVC films. The level of DEHP and DEHA in samples was determined by leaving the film in contact with n-heptane during 48 hours and analysis in a gas chromatograph (GC) equipped with a flame ionization detector and fused silica column with 5% phenylmethyl silicone in the dimensions 30 m x 0.53 mm x 2.65 mm. The results for detection and the quantification limits were smaller than the restriction limits. The recovery rates of DEHP and DEHA were, respectively, 69.10 ...