A hydrometallurgical process applicable to printed circuit boards of small electrical and electronic devices was developed. This involved three leaching steps (60 ºC, 2 h): 6 mol L-1 NaOH, 6 mol L-1 HCl and aqua regia. NaOH removed the resin and flame retardant that covered the circuit boards. HCl dissolved the most electropositive metals and a small amount of copper (~0.3 wt%). Aqua regia dissolved the noble metals. Silver precipitated as AgCl. Gold and platinum were quantitatively extracted with pure methyl-isobutylketone and Alamine 336 (10 % vol. in kerosene), respectively. Slow evaporati...