Molecular and morphological surface analysis: effect of filling pastes and cleaning agents on root dentin
Abstract The quality of the dentin root is the most important factor for restoration resin sealing and drives the outcome of endodontic treatment. Objective This study evaluated the effect of different filling pastes and cleaning agents on the root dentin of primary teeth using Fourier-transformed Raman spectroscopy (FT-Raman), micro energy-dispersive X-ray fluorescence (µ-EDXRF) and scanning electron microscopic (SEM) analysis. Material and Methods Eighty roots of primary teeth were endodontically prepared and distributed into 4 groups and filled according to the following filling pastes...