Mechanical properties and fractography of cement-based composites reinforced by natural piassava and jute fibers
Abstract Today’s demand for environmentally friendly and energy-efficient solutions to the construction industry has driven researchers to match natural resources with traditional technics to develop new building technologies. However, there are literature limitations about the correlation of fiber-matrix interface with the failure of natural fibers in mortar plates, which hinders the advances in understanding the mechanical properties of these composites on a structural scale. The present work investigated the mechanical behavior and fractography of cement-based composites reinforced by nat...