Fractographic and rheological characterizations of CF/PP-PE-copolymer composites tested in tensile
Abstract This work shows the fractographic study of fractured surfaces resulted from tensile tests of thermoplastic composites based on poly(propylene-co-ethylene) (PP-PE) and modified PP-PE copolymers reinforced with continuous carbon fibers (CF). The PP-PE matrix was modified with two agents called AM1 (based on maleic anhydride) and AM2 (containing an elastomeric agent), respectively. Three different laminates - CF/PP-PE, CF/PP-PE(AM1) and CF/PP-PE(AM2) - were manufactured. The best tensile strength and elastic modulus results were determined for the CF/PP-PE(AM1) laminate (507.6 ± 11.8 MP...