Effect of Quenching Rate and Pre-strain on the Strain Ageing Behaviors of 7075 Aluminum Alloys

The mechanical properties of aluminum alloys are strongly dependent on the thermo-mechanical process so, the strain ageing behavior of 7075 Al-alloy was investigated in this study. A set of test pieces was solution heat treated at 480 °C for 2 h, water quenched (SHTWQ) then pre-strained for 8% in tension. The test samples were aged at 140 °C for 0.5, 1, 2, 3, 4, 6, 8, 10, 12, 24, 48, 72 and 96 h in a furnace. The other set of test samples were solution heat treated at 480 °C for 2 h, quenched in sand (SHTSQ) then pre-strained for 8% in tension. They were also aged at 140 °C for same interv...