1. Mechanical properties and fractography of cement-based composites reinforced by natural piassava and jute fibers
Abstract Today’s demand for environmentally friendly and energy-efficient solutions to the construction industry has driven researchers to match natural resources with traditional technics to develop new building technologies. However, there are literature limitations about the correlation of fiber-matrix interface with the failure of natural fibers in mor
Cerâmica. Publicado em: 2022
-
2. Mechanical and Metallurgical Characterization of Laser Welding on P91 Ferritic Steel and Incoloy 800HT Dissimilar Joints
In this work, microstructural characterization and mechanical properties of P91 and Incoloy 800HT dissimilar laser beam welded joint were analyzed. In addition to that, metallographical studies were conducted using Optical microscopy, Scanning electron microscopy (SEM) equipped with Energy-dispersive X-ray spectroscopy (EDX) and X-Ray diffraction analysis (
Mat. Res.. Publicado em: 01/02/2018
-
3. Effect of Boride Layer on PM HSS AISI M2 on the Mechanisms Acting in the Transverse Rupture Strength Test
Herein, it was conducted a study in order to examine the main fracture characteristics in the transverse rupture strength test (TRS) of a high speed steel (HSS) AISI M2 produced by powder metallurgy (PM) and with boriding treatment. Four conditions have been studied: as-sintered, borided, normalized and borided + TiN. The TRS tests were conducted in accordan
Mat. Res.. Publicado em: 06/11/2017
-
4. The effect of cold forming on structure and properties of 32 CDV 13 steel by radial forging process
The present study focuses on the effect of various degrees of plastic deformation generated by cold radial forging on the mechanical properties and the fracture morphology of 32 CDV 13 steel. The cold forging percentage was evaluated for 17.45, 33.30, 42.0 and 46.47 %. The microstructural analysis of the steel shows tempered martensite. The tensile strength,
Mat. Res.. Publicado em: 01/04/2014
-
5. Normalizing effect on fatigue crack propagation at the heat-affected zone of AISI 4140 steel shielded metal arc weldings
The fractography and mechanical behaviour of fatigue crack propagation in the heat-affected zone (HAZ) of AISI 4140 steel welded using the shielded metal arc process was analysed. Different austenitic grain size was obtained by normalizing performed at 1200 °C for 5 and 10 hours after welding. Three point bending fatigue tests on pre-cracked specimens along
Mat. Res.. Publicado em: 02/04/2013
-
6. Efeitos do revenimento realizado a baixa temperatura na resistência ao impacto em aços carbono e ligados temperados
This work has as main objective the determination of mechanical behavior, specially the impact resistance of martensitic structures based on carbon and on alloyed steels. The main concern is the response of these alloys when tempering at low temperatures (below 180C). Heat treatments were performed by quenching in water and oil in order to determine the seve
IBICT - Instituto Brasileiro de Informação em Ciência e Tecnologia. Publicado em: 15/02/2011
-
7. Mechanical behavior of ceramic materials used for fixed partial dentures / Comportamento mecânico de cerâmicas utilizadas na confecção de próteses parciais fixas
Objectives: to determine the flexural strength (f), Weibull modulus (m), slow crack growth coefficient (n) and fracture toughness (KIC) of three ceramics used as framework materials for fixed partial dentures (FPDs) (YZ- yttria partially stabilized zirconia tetragonal polycrystals; IZ- alumina-based zirconia-reinforced glass infiltrated ceramic; AL alumina p
Publicado em: 2010
-
8. Mechanical properties of commercially pure titanium and Ti-6Al-4V alloys casting in different environments / Propriedades mecânicas do titânio comercialmente puro e da liga Ti-6Al-4V fundidos em diferentes ambientes
Background: Although CP titanium and titanium alloys have been used for medical and dental applications, their high cost has not stimulated their current use. Objective: The purpose of this study was to evaluate the effect of argon purity on the mechanical properties, microstructure and fractography of CP Ti (Grade I) and Ti-6Al- 4V cast alloys. Material and
Publicado em: 2007
-
9. Resistencia mecanica e tenacidade a fratura do osso cortical bovino / Mechanical strength and fracture toughness of cortical bovine bone
Stress fractures are caused by fatigue exercising in bones that occur in young health people who are submitted to rigorous physical training. It?s known that its path physiology is characterized by initiation and propagation of microcracks. Thus, the purpose of this study is to identify some of the mechanical properties of cortical bone that approach to the
Publicado em: 2006
-
10. Estudo da influência do meio corrosivo na resistência à fadiga do aço estrutural SAE 8620
A corrosão-fadiga é provavelmente um dos mais complexos de todos os fenômenos, sendo influenciada por fatores ambientais, mecânicos, metalúrgicos, somados a uma componente cíclica de tensões. A corrosão-fadiga pode ser definida como a ação combinada de um ambiente agressivo e uma tensão cíclica que conduzem à falha prematura dos metais por trinc
Publicado em: 2006
-
11. FATIGUE BEHAVIOR OF CEMENTITIOUS COMPOSITES REINFORCED BY BAMBOO PULP / COMPORTAMENTO EM FADIGA DE COMPÓSITOS CIMENTÍCIOS REFORÇADOS POR POLPA DE BAMBU
A utilização de materiais de construção civil a base de cimento reforçado com fibras vem aumentando rapidamente nos últimos anos. No Brasil um vasto programa experimental para avaliar o comportamento mecânico desses materiais através de ensaios de flexão monotônicos e de compressão, vem sendo desenvolvidos na PUC/RIO desde 1979. Este trabalho proc
Publicado em: 2006
-
12. Uma metodologia para a avaliação dos gradientes de tenacidade a fratura ao longo da camada cementada do aço SAE 5115 / A model for fracture toughness evaluation of the carburized layer for SAE 5115 steel
The purpose of this work is to propose a model for evaluating the fracture toughness along the SAE 5115 steel carburized layer. Due to the small thickness of those layers, it is impossible to machine specimens from those layer in accordance with standards. For simulating the microstructures of the carburized layer in order to get samples for tensile and the
Publicado em: 2005