The objective of the present study was to evaluate the adsorption of the herbicide Diuron onto smectite and Fe oxides minerals. Ninety mg of each mineral, 1 mL of 0.15 mol L-1 CaCl2 and 8 mL of Diuron (0.25-10.00 mg L-1) were used in triplicates. These materials were shaken, ultra centrifuged and the supernatant collected and analysed on a UV-Vis spectrophotometer. The Diuron presented low adsorption onto clay mineral fractions. Adsorption was greater onto Fe oxides at pH 7.0, possibly due to proximity to the point of zero charge of these minerals.