Processamento de catalisadores gastos de unidade de hidrodessulfurização profunda (ultra-deep HDS)

AUTOR(ES)
FONTE

Química Nova

DATA DE PUBLICAÇÃO

2022

RESUMO

PROCESSING OF SPENT ULTRA-DEEP HYDRODESULFURIZATION CATALYSTS. This work discusses the recycling of spent NiMo/Al2O3 catalysts from ultra-deep hydrodesulfurization (HDS) units. They contain a refractory coke and fouling elements from the processed feedstocks. Samples were preoxidized (600 ºC) for 12 h using a very slow heating rate to eliminate coke and volatiles. Experiments were performed in the presence of HF + H2O2 mixtures under stirring at 25-60oC for 1-4 h. The amount of insoluble matter was the lowest (< 1 wt.% of the initial mass) after leaching for 2 h at 60oC using an excess of 50 vol.% HF and 20 vol.% H2O2. Leached molybdenum and vanadium were extracted together with Alamine 304 (tri-dodecylamine) in n-heptane at pH below 2. Aluminum and iron were precipitated from the raffinate as Na3AℓF6 (+ Na3FeF6) by adjusting pH at ~4 using 6 mol L-1 NaOH. Nickel was either recovered by solvent extraction using D2EHPA (bis-(2-ethylhexyl)phosphoric acid) in n-heptane at pH 6 or precipitated at pH 8 using 6 mol L-1 NaOH. The first method proved better as less contaminants were present. After slow evaporation of the final aqueous solution, a mixture of Na2SiF6 and NaF was recovered. Fluoride losses were very low (~0.10 wt.%).

Documentos Relacionados