The development of new ceramic systems creates the possibility of choice above the type of restoration one could mean to choose. Thus, benefits from this progress must be appraised on the possibility of unsatisfactory clinical behavior. This work intends to evaluate ceramic copings to the influence of internal adjustment on adaptation, vertical misfit after cementation, film thickness of axial and occlusal surfaces and occurrence of oblique seating. A metallic superior premolar analogue with full crown preparation was yield and thirty casts were obtained and divided into three groups of ten specimens each. Metal copings were yield for group MC and ceramics copings of In-Ceram Zirconia and Procera AllZircon were yield for group IZ and group PZ, respectively. The copings had their position, in relation to the metallic analogue, measured during adjustment and cementation with light body silicon. Cement film, below the copings, was sectioned and measured at the axial and occlusal surfaces. The analysis of the results demonstrated that: 1) internal adjustment of metal and In-Ceram Zirconia copings reduced the vertical misfit; 2) vertical misfit after cementation of Procera AllZircon copings was statistically different from metal and In-Ceram Zirconia copings; 3) film thickness of Procera AllZircon copings was significantly greater than metal and In-Ceram Zirconia copings; 4) all copings presented oblique seating.

ASSUNTO(S)

desajuste vertical film thickness sistemas cerâmicos vertical misfit ceramic systems cimentação. cementation espessura de película

Documentos Relacionados