Evaluation of degree of conversion, microtensile bond strength and mechanical properties of three etch-and-rinse dental adhesives
AUTOR(ES)
Freitas, Samantha Ariadne Alves de, Lanza, Marco Daniel Septimo, Carneiro, Karina Kato, Loguercio, Alessandro Dourado, Bauer, José
FONTE
Polímeros
DATA DE PUBLICAÇÃO
21/09/2017
RESUMO
Abstract This study evaluated microtensile bond strength (µTBS), degree of conversion, modulus of elasticity and ultramicrohardness of three etch-and-rinse adhesives systems. The materials evaluated were: Ambar (FGM), Optibond (Kerr) and Magic Bond (Vigodent). The degree of conversion was analyzed by FTIR/ATR. To evaluate bond strength (μTBS) in dentin, 15 teeth (n = 5) were restored and sliced to obtain the specimens (0.8mm2). The dynamic ultra microhardness tester was used to evaluate the hardness and modulus of elasticity. The Magic Bond adhesive system showed lower µTBS than Ambar and Optibond (p <0.001). For degree of conversion, comparisons between groups of adhesive systems evaluated showed statistically significant difference (p<0.001), with higher values for Ambar and Optibond when compared a Magic Bond. For modulus of elasticity and ultramicrohardness, Ambar and Magic Bond showed lower values than Optibond. The best results in all properties evaluated were obtained by the Optibond adhesive system.
Documentos Relacionados
- Bond Stability of Universal Adhesives Applied To Dentin Using Etch-And-Rinse or Self-Etch Strategies
- Effect of tetracycline on the bond performance of etch-and-rinse adhesives to dentin
- EFEITO DA DOXICICLINA NA RESISTÊNCIA DE UNIÃO À DENTINA DE UM SISTEMA ADESIVO ETCH-AND-RINSE
- Bond strength assessment of a universal adhesive system in etch-and-rinse and self-etch modes
- Effect of surface area and air-drying distance on shear bond strength of etch-and-rinse adhesive